The spraying process of automotive paint is generally divided into several processes: primer, intermediate coating, topcoat, and varnish. During the spraying process, it is inevitable to encounter one or more problems. Changzhou Wante Coatings has compiled ten common problems and solutions for automotive paint.
Common problem 1: Orange peel on the paint surface
Reason for composition:
1. Incorrect spraying pressure, viscosity, spraying method or construction temperature,
2. Improper use of curing agents and diluents;
3. Insufficient polishing of the substrate;
4. The car paint is not well mixed
Solution:
1. Strictly adjust the spray gun pressure according to technical data, use the correct spraying method and construction temperature, and avoid construction at very high or very low temperatures;
2. The curing agent and diluent are proportioned according to the correct ratio;
3. Correct polishing of the substrate;
4. Mix the paint thoroughly before use
Common problem 2: Solvent bubbles (prickly heat, hot prickly heat)
Reason for composition:
1. The paint film is sprayed too thick
2. Improper use of curing agents and diluents leads to rapid drying
Solution:
1. Correct use of spray gun and spray viscosity
2. Use appropriate curing agents and diluents to avoid appearing too dry and fast
Common problem three: pinholes
Reason for composition:
1. The substrate is made of glass fiber, which easily forms pinholes;
2. Insufficient mixing and priming of atomic ash;
3. There are solvent bubbles on the surface after polishing
Solution:
1. Mix all atomic ashes and fill with enough atomic ashes
2. Do not polish solvent bubbles
3. Remove all the problematic paint film thoroughly
4. Remove the problematic paint surface, polish it from the beginning, apply atomic ash, and then spray the topcoat from the beginning
Common Question 4: Color Deviation
Reason for composition:
1. Insufficient mixing of paint before application
2. Incorrect spraying method, uneven spraying thickness
3. Inaccurate color matching
Solution:
1. Mix thoroughly and evenly before opening the tank for use
2. Apply the correct spraying method and dilution ratio to achieve uniform spraying
3. Accurate color matching
FAQ 5: Blistering
Reason for composition:
1. Mainly due to insufficient drying or cleaning of the substrate before spraying, which contains moisture and oil stains
Solution:
1. All materials must be properly dried before construction;
2. Fully clean the substrate
Article source: Qingyuan Automotive Repair Painthttp://www.jinliangxincai.com
08-25
Common problems with automotive repair paint
Why are the orange lines on the surface of the varnish so heavy after each spray? Why on earth? How can we prevent a decrease?Answer: The thinness of the varnish, the amount of paint produced by the s
06-05
The car repair paint manufacturer told you about the problem with water-based coatings
1. How long does it take for a skilled paint coating technician to master the operation of water paint?Generally, practice and understanding with less than half a sound can be mastered, and proficienc
05-31
Qingyuan Automobile Repair Paint Company tells you the steps for painting
Automotive Painting Process(1) Rust prevention and internal painting of the vehicle body: Depending on the condition of the vehicle body, it will be completed by a sheet metal worker.(2) Polishing and
05-12
Why does car repair paint lack luster?
If there is a lack of gloss on the surface of the originally flat and smooth car paint surface, especially during the process of car paint care, it can be observed under a microscope that the surface