When it comes to the shortcomings of car paint, I believe most car owners hope to quickly repair them to prevent more serious problems from appearing, and also to not affect the appearance of the car. So, what are the methods for quickly repairing car paint? In terms of rapid repair of car paint, it is also necessary to select corresponding methods based on different scratch conditions, as detailed below:
1、 When the car's paint surface shows a loss of gloss, it can be restored by using a high-speed polishing machine in conjunction with a specialized abrasive for polishing treatment, and it will not show a loss of gloss in the future.
2、 Echo bite paint. Due to the non drying of the site and the wet spraying during spraying, it may be due to the self spraying of the garden spray, as well as the chemical reaction caused by the use of inferior car paint during spraying, which can cause paint biting. When there is paint biting, the area should be dried with an iodine tungsten lamp first, and then the biting area should be polished smooth with P1500-P2000 water sanding paper. After drying, the paint can continue to be sprayed. If there is still a reaction, the original paint should be completely removed, and a new base should be made before spraying.
3、 The orange lines are too large. If the air pressure is too high or if the gun is driven too fast, it may cause orange lines to increase. When the air pressure is adjusted at 2Kpa, it should be slow to move the gun, and it can be compacted by half and stacked for spraying. If orange lines are found after baking, polish and polish them.
4、 Color difference. Before spraying, special colors should be tested and confirmed to be correct before spraying. When repairing, the original paint should be preserved to the maximum extent possible under the spraying requirements. Excessive repair can be used to solve the color difference problem.
5、 Tears and dirty spots. Regarding the appearance of tears and dirty spots after spraying, polishing can be used. Use a small pad with a hard surface and P1500 water sandpaper to polish, then use a soft surface to polish, and then polish after leveling.
Article source: Automotive repair paint http://www.jinliangxincai.com
08-25
Common problems with automotive repair paint
Why are the orange lines on the surface of the varnish so heavy after each spray? Why on earth? How can we prevent a decrease?Answer: The thinness of the varnish, the amount of paint produced by the s
06-05
The car repair paint manufacturer told you about the problem with water-based coatings
1. How long does it take for a skilled paint coating technician to master the operation of water paint?Generally, practice and understanding with less than half a sound can be mastered, and proficienc
05-31
Qingyuan Automobile Repair Paint Company tells you the steps for painting
Automotive Painting Process(1) Rust prevention and internal painting of the vehicle body: Depending on the condition of the vehicle body, it will be completed by a sheet metal worker.(2) Polishing and
05-12
Why does car repair paint lack luster?
If there is a lack of gloss on the surface of the originally flat and smooth car paint surface, especially during the process of car paint care, it can be observed under a microscope that the surface